Grain-size-resolved defect modelling and interface optimisation in 2D/3D/2D perovskite solar cells: a numerical study


Rajabi-Ghaleh S., Kheradmand R., Ahmadi-Kandjani S., OLYAEEFAR B., Fathalizadeh N.

Physica Scripta, cilt.101, sa.41, 2026 (SCI-Expanded, Scopus)

  • Yayın Türü: Makale / Tam Makale
  • Cilt numarası: 101 Sayı: 41
  • Basım Tarihi: 2026
  • Doi Numarası: 10.1088/1402-4896/aeaf1e
  • Dergi Adı: Physica Scripta
  • Derginin Tarandığı İndeksler: Science Citation Index Expanded (SCI-EXPANDED), Scopus, Chemical Abstracts Core, Compendex, INSPEC, zbMATH
  • Anahtar Kelimeler: and perovskite solar cell, defect density, Grain size, interface, Matthiessen’s rule
  • Orta Doğu Teknik Üniversitesi Adresli: Evet

Özet

Grain boundary defect density and interfacial recombination are the two dominant loss mechanisms limiting perovskite solar cell performance, yet they are rarely optimised within a unified theoretical framework. Here, we extend the corrected Matthiessen’s rule formulation for grain-size-dependent defect density—originally established for three-dimensional (3D) perovskites in our prior work (Olyaeefar et al 2018 Sol. Energy Mater. Sol. Cells 180 76–82) to two-dimensional (2D) perovskite systems, accounting for the 2D adaptation of the corrected Matthiessen’s rule framework consists primarily of a revised grain-boundary defect density (Formula presented) (Formula presented). The resulting grain-size-resolved defect densities are used directly as inputs to drift-diffusion simulations in (Formula presented) (Formula presented), establishing a physically consistent link between film microstructure and device behaviour. Photoluminescence quantum yield analysis confirms that 2D perovskites exhibit higher radiative efficiency at small grain sizes due to strong excitonic confinement, and the extracted recombination coefficients constrain the defect density parameters used in simulation. Five device architectures—single-layer 3D, 2D/3D, 2D/I/3D, 2D/3D/2D, and 2D/I/3D/I/2D—are systematically compared under identical modelling conditions. The 3D baseline (Formula presented) (Formula presented) is calibrated against and validated by experimental data. The optimised 2D/I/3D/I/2D architecture, incorporating quasi-2D Ruddlesden–Popper interlayers at both 2D/3D interfaces, achieves a simulated PCE of (Formula presented) (Formula presented), with (Formula presented) (Formula presented) and (Formula presented) (Formula presented), improvements attributed to suppressed trap-assisted recombination and enhanced charge extraction at engineered interfaces. This work provides a transferable framework for simultaneously optimising grain structure and interface design in multi-dimensional perovskite photovoltaics.